Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 16.3 J @Temperature -40.0 °C |
12.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech CamAlloy /ABS Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 16.3 J @Temperature -40.0 °C |
12.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech Korad® SP-9011 Cap ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 16.3 J @Temperature -40.0 °C |
12.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech SP-9010 General Purpose ABS Sheet Description: ABS SheetInformation provided by Spartech. |