Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech CamAlloy /ABS Weatherable Sheet

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Spartech
Trade Name CamAlloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech CamAlloy /ABS Weatherable Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Weatherable SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Unnotched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
1.33 J/cm

@Temperature -40.0 °C
2.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 44.7 J
33.0 ft-lb
73°F; ASTM D3029
16.3 J

@Temperature -40.0 °C
12.0 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: