Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 159 J | 117 ft-lb | Falling weight impact at 23°C (73.4°F) |
Kraton® D1102 + PP blend (10/90) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |