Mechanical Properties Metric English Comments
Falling Dart Impact 2.17 - 18.6 J
1.60 - 13.7 ft-lb
Average value: 10.7 J Grade Count:4
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Falling Dart Impact 2.17 J
1.60 ft-lb
Kolon DIAMAT® GP
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..