Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop, Total Energy = 56.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer
18 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Europe-Africa-Middle East)
18 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer
18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific)
18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East)
18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific)
18 MFR LEXAN High Flow Ductile Copolymer
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
Dart Drop, Total Energy 76.0 J

@Temperature 23.0 °C
56.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0
Dart Drop, Total Energy 76.0 J
56.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant.
Dart Drop, Total Energy 76.0 J
56.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact.
Dart Drop, Total Energy 76.0 J
56.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Dart Drop, Total Energy 76.0 J
56.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Dart Drop, Total Energy 76.0 J
56.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved