Mechanical Properties Metric English Comments
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER
LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific)
LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Europe-Africa-Middle East)
LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER
LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Asia Pacific)
LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Asia Pacific)
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Europe-Africa-Middle East)
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HP1HF PC
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East)
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML3729 PC
Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing.
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Europe-Africa-Middle East)
LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific)
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER
Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER
Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific)
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Asia Pacific)
Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® ML1661 PC Copolymer (Asia Pacific)
Medium-flow impact-modified light-shielding high-flow-ductile PC copolymer. Available in white color only.
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Asia Pacific)
Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm..
Dart Drop, Total Energy 66.0 J

@Temperature 23.0 °C
48.7 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER
Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U..