Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Asia Pacific) Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm .. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML3729 PC Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Asia Pacific) Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML1661 PC Copolymer (Asia Pacific) Medium-flow impact-modified light-shielding high-flow-ductile PC copolymer. Available in white color only. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Asia Pacific) Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
Dart Drop, Total Energy | 66.0 J @Temperature 23.0 °C |
48.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |