Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 45.0 - 45.0 J @Temperature -20.0 - -20.0 °C |
33.2 - 33.2 ft-lb @Temperature -4.00 - -4.00 °F |
Average value: 45.0 J Grade Count:1 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |