Mechanical Properties Metric English Comments
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU
LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant.
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DX98477 PC
LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
Dart Drop, Total Energy 45.0 J

@Temperature -20.0 °C
33.2 ft-lb

@Temperature -4.00 °F
DIN 53443
Zell-Metall Engineering Plastics Zellamid 202 (PA 6)
Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased...
Dart Drop, Total Energy 45.0 - 45.0 J

@Temperature -20.0 - -20.0 °C
33.2 - 33.2 ft-lb

@Temperature -4.00 - -4.00 °F
Average value: 45.0 J Grade Count:1
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Dart Drop, Total Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications