Dart Drop, Total Energy 40.1 J
29.6 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ 5101-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding ..
Dart Drop, Total Energy 40.1 J
29.6 ft-lb
3.39 m/sec; ASTM D3763
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin
Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL..