Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 10.0 - 33.0 J @Temperature -30.0 - -30.0 °C |
7.38 - 24.3 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 21.0 J Grade Count:9 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |