Mechanical Properties Metric English Comments
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific)
High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi.
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4504 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific)
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4701R PPC
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific)
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4704 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4704 PPC (Asia Pacific)
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J

@Temperature 23.0 °C
110 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Lexan® HPH4504 PPC
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Dart Drop, Total Energy 149 J

@Temperature 23.0 °C
110 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4704 PPC
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4704 PPC (Asia Pacific)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J

@Temperature 23.0 °C
110 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Lexan® PPC4504 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit..
Dart Drop, Total Energy 149 J

@Temperature 23.0 °C
110 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Lexan® PPC4701 PPC
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi.This data was supplied by SABIC-IP for the Americas region.
Dart Drop, Total Energy 149 J

@Temperature 23.0 °C
110 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Lexan® PPC4701R PPC
High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
Dart Drop, Total Energy 149 J

@Temperature 23.0 °C
110 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Lexan® PPC4704 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® 4501 PPC
High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi.
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril..
Dart Drop, Total Energy 149 - 169 J
110 - 125 ft-lb
Average value: 154 J Grade Count:4
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Dart Drop, Total Energy 149 J

@Temperature 23.0 °C
110 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Lexan® ML5472 PC
Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region.
Dart Drop, Total Energy 149 J
110 ft-lb
ASTM D3029
SABIC Innovative Plastics Lexan® HPH4504H PPC
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
Copyright © lookpolymers.com All Rights Reserved