Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 40.0 MPa | 5800 psi | |
Wolf Kunststoff ZEDEX® ZX-100A Polymer Alloy Main Characteristics: Tough; Resilient; Soft; Low cost solutionApplications: Handling, Vessel and pump, Steel and Water, Chemical Engineering, Automitve Technology, Machine ToolsInformation provided.. |
|||
Fatigue Strength | 40.0 MPa @# of Cycles 1.00e+6 |
5800 psi @# of Cycles 1.00e+6 |
1 Hz |