Polymer Property : Fatigue Strength = 40.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength 40.0 MPa
5800 psi
Wolf Kunststoff ZEDEX® ZX-100A Polymer Alloy
Main Characteristics: Tough; Resilient; Soft; Low cost solutionApplications: Handling, Vessel and pump, Steel and Water, Chemical Engineering, Automitve Technology, Machine ToolsInformation provided..
Fatigue Strength 40.0 MPa

@# of Cycles 1.00e+6
5800 psi

@# of Cycles 1.00e+6
1 Hz
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..