Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 21.0 MPa @# of Cycles 1.00e+7 |
3050 psi @# of Cycles 1.00e+7 |
ASTM D-671 |
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p.. |