Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 206.5 MPa @Temperature 20.0 °C |
29950 psi @Temperature 68.0 °F |
P50% rotary bending values for 5X10<sup>7</sup> cycles |
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |