Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 186 MPa @# of Cycles 5.00e+7 |
27000 psi @# of Cycles 5.00e+7 |
Axial; R = 0.1; Extruded Bar; ASTM E466 |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |