Polymer Property : Ball Indentation Hardness = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa

@Load 36.5 kg
13100 psi

@Load 80.5 lb
cond.; ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 CFHI Polyamide 6 - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..