Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 85.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 7.89 - 14.9 kN/m

@Temperature 91.0 °C
45.0 - 85.0 pli

@Temperature 196 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Copyright © lookpolymers.com All Rights Reserved