Mechanical Properties Metric English Comments
Peel Strength 7.89 - 14.9 kN/m

@Temperature 91.0 °C
45.0 - 85.0 pli

@Temperature 196 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF/SW, MIL-C-5541
3M AC-350 Class C-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF, AMS 4911 Titanium
3M AC-350 Class C-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 6.05e+6 sec
45.0 pli

@Temperature 140 °F,
Time 1680 hour
in JRF/SW, AMS 4911 Titanium
3M AC-350 Class C-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF, MIL-PRF-85582
3M AC-350 Class C-1/2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF/SW, MIL-C-5541
3M AC-350 Class C-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF, AMS 4911 Titanium
3M AC-350 Class C-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 6.05e+6 sec
45.0 pli

@Temperature 140 °F,
Time 1680 hour
in JRF/SW, AMS 4911 Titanium
3M AC-350 Class C-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF, MIL-PRF-85582
3M AC-350 Class C-2 Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF/SW, MIL-C-5541
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF, AMS 4911 Titanium
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 6.05e+6 sec
45.0 pli

@Temperature 140 °F,
Time 1680 hour
in JRF/SW, AMS 4911 Titanium
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..
Peel Strength 7.89 kN/m

@Temperature 60.0 °C,
Time 605000 sec
45.0 pli

@Temperature 140 °F,
Time 168 hour
in JRF, MIL-PRF-85582
3M AC-350 Class C-8(24) Aerospace Sealant
3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav..