Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 8.94 kN/m @Temperature 24.0 °C, Time 432000 sec |
51.0 pli @Temperature 75.2 °F, Time 120 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Peel Strength | 8.94 kN/m @Temperature 24.0 °C, Time 432000 sec |
51.0 pli @Temperature 75.2 °F, Time 120 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |