Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 8.59 kN/m @Temperature -34.0 °C, Time 1.81e+6 sec |
49.0 pli @Temperature -29.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Peel Strength | 8.59 kN/m @Temperature -34.0 °C, Time 1.81e+6 sec |
49.0 pli @Temperature -29.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |