Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 12.8 kN/m @Temperature 24.0 °C |
73.0 pli @Temperature 75.2 °F |
Metal-to-metal |
Hexcel® HexPly® F185 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F185; Fiber: 150-1/2Information provided by HexCel |