Mechanical Properties Metric English Comments
Peel Strength 25.4 kN/m

@Temperature 113 °C
145 pli

@Temperature 235 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers