Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film

Category Polymer , Film , Thermoplastic , Polyurethane, TP
Manufacturer Huntsman Corporation
Trade Name KRYSTALFLEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength at Break 46.9 MPa
6800 psi
ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
100% Modulus 0.00758 GPa
1.10 ksi
ASTM D412
300% Modulus 0.0262 GPa
3.80 ksi
ASTM D412
Tear Strength 75.4 kN/m
430 pli
ASTM D624
Peel Strength 6.84 kN/m

@Temperature 91.0 °C
39.0 pli

@Temperature 196 °F
resistance to glass; ASTM D3167
19.3 kN/m

@Temperature 99.0 °C
110 pli

@Temperature 210 °F
resistance to glass; ASTM D3167
25.4 kN/m

@Temperature 113 °C
145 pli

@Temperature 235 °F
resistance to glass; ASTM D3167
27.2 kN/m

@Temperature 118 °C
155 pli

@Temperature 244 °F
resistance to glass; ASTM D3167
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -64.0 °C
-83.2 °F
Processing Properties Metric English Comments
Melt Temperature 94.0 - 144 °C
201 - 291 °F