Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 10.4 kN/m @Temperature 82.0 °C |
59.3 pli @Temperature 180 °F |
Metal-to-metal |
Hexcel® HexPly® F185 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F185; Fiber: 450-1/2Information provided by HexCel |