Material Notes:
Hexcel designation: 120-38"-F185; Fiber: 450-1/2Information provided by HexCel
Physical Properties Metric English Comments
Volatiles 0.40 - 1.2 %
0.40 - 1.2 %
Prepreg
Mechanical Properties Metric English Comments
Tensile Strength, Yield 308 MPa

@Temperature 24.0 °C
44700 psi

@Temperature 75.2 °F
Warp TS
Compressive Yield Strength 283 MPa

@Temperature 24.0 °C
41000 psi

@Temperature 75.2 °F
Warp compression
Shear Strength 26.676 MPa

@Temperature 82.0 °C
3869.0 psi

@Temperature 180 °F
Lap shear
34.246 MPa

@Temperature -54.0 °C
4967.0 psi

@Temperature -65.2 °F
Lap shear
35.432 MPa

@Temperature 24.0 °C
5139.0 psi

@Temperature 75.2 °F
Lap shear
Peel Strength 6.95 kN/m

@Temperature -54.0 °C
39.7 pli

@Temperature -65.2 °F
Metal-to-metal
8.72 kN/m

@Temperature 24.0 °C
49.8 pli

@Temperature 75.2 °F
Metal-to-metal
10.4 kN/m

@Temperature 82.0 °C
59.3 pli

@Temperature 180 °F
Metal-to-metal
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.012
Laminate
Fiber Volume (%) 36.1
Laminate
Flow (%) 24-34
Wet Resin Content (%) 57-63
Prepreg