Polymer Property : Tensile Strength = 8410 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 58.0 MPa

@Temperature 150 °C
8410 psi

@Temperature 302 °F
ASTM D638
DuPont Performance Polymers VESPEL TP-8054 Polyimide
DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi..
Tensile Strength 58.0 MPa

@Temperature 23.0 °C
8410 psi

@Temperature 73.4 °F
5mm/min (0.2in/min); ASTM D638
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..