Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 58.0 MPa @Temperature 150 °C |
8410 psi @Temperature 302 °F |
ASTM D638 |
DuPont Performance Polymers VESPEL TP-8054 Polyimide DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyi.. |
|||
Tensile Strength | 58.0 MPa @Temperature 23.0 °C |
8410 psi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |