Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 655 MPa @Thickness 4.762 - 12.7 mm |
>= 95000 psi @Thickness 0.1875 - 0.500 in |
ASTM E-8 |
H.C. Starck 3203 Pure Molybdenum APL, Arc-Cast, Low Carbon Plate Arc-Cast Plate 3203 Low CarbonDescription of Product: This specification covers rolled plate of carbon-deoxidized molybdenum produced from ingots consolidated by the H.C. Starck consumable electrod.. |