Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 425 MPa @Thickness 152.4 - 203.2 mm |
61600 psi @Thickness 6.000 - 8.000 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength | >= 425 MPa @Thickness 15.0 - 38.1 mm |
>= 61600 psi @Thickness 0.591 - 1.50 in |
Tempers T651 / T652 |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |