Mechanical Properties Metric English Comments
Tensile Strength 425 MPa

@Thickness 152.4 - 203.2 mm
61600 psi

@Thickness 6.000 - 8.000 in
Typical Strength
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength >= 425 MPa

@Thickness 15.0 - 38.1 mm
>= 61600 psi

@Thickness 0.591 - 1.50 in
Tempers T651 / T652
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..