Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 385 MPa @Thickness 40.0 - 60.0 mm |
>= 55800 psi @Thickness 1.57 - 2.36 in |
Temper T451; Standard EN 485-2 |
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the.. |