Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 26.0 - 30.0 MPa @Temperature 50.0 °C |
3770 - 4350 psi @Temperature 122 °F |
|
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,.. |