Mechanical Properties Metric English Comments
Tensile Strength 415 MPa

@Thickness 7.90 - 25.0 mm
60200 psi

@Thickness 0.311 - 0.984 in
Typical Strength; Standard EN 485-2
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Tensile Strength 415 MPa

@Thickness 25.0 - 60.0 mm
60200 psi

@Thickness 0.984 - 2.36 in
Typical Strength; Standard EN 485-2
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Tensile Strength 415 MPa

@Thickness 60.0 - 155 mm
60200 psi

@Thickness 2.36 - 6.10 in
Typical Strength; Standard EN 485-2
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..
Tensile Strength >= 415 MPa

@Thickness 38.1 - 76.2 mm
>= 60200 psi

@Thickness 1.50 - 3.00 in
Tempers T651 / T652
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength >= 415 MPa

@Thickness 76.2 - 127 mm
>= 60200 psi

@Thickness 3.00 - 5.00 in
Tempers T651 / T652
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength 415 MPa

@Thickness 35.0 - 60.0 mm
60200 psi

@Thickness 1.38 - 2.36 in
Typical Strength
Constellium Unidal® High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Unidal® precision plates offers a combination of dimensional stability and high mechanical strength. The very low internal stress reduces the risk of deformation during machining, thereby reducing ..