Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 250 MPa @Diameter 80.0 - 150 mm |
36300 psi @Diameter 3.15 - 5.91 in |
|
United Cast Bar Unibar 350 Continuously Cast Iron Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a.. |