Mechanical Properties Metric English Comments
Tensile Strength 250 MPa

@Diameter 80.0 - 150 mm
36300 psi

@Diameter 3.15 - 5.91 in
United Cast Bar Unibar 350 Continuously Cast Iron
Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a..