Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 120 MPa @Strain 3.00 %, Temperature 80.0 °C |
17400 psi @Strain 3.00 %, Temperature 176 °F |
5mm/min |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Tensile Strength | 120 MPa @Temperature 23.0 °C |
17400 psi @Temperature 73.4 °F |
ISO 527 |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
Tensile Strength | 120 MPa @Temperature 50.0 °C |
17400 psi @Temperature 122 °F |
ISO 527 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |