Polymer Property : Izod Impact, Unnotched (ISO) = 77.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 77.0 kJ/m²

@Temperature 23.0 °C
36.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber
SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers