Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 77.0 kJ/m² @Temperature 23.0 °C |
36.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXAMID 126F5 Nylon 6, 25% Glass Fiber SAXAMID 126F5 is a polyamide 6 injection-molding-grade reinforced with 25% glass fibers.Information provided by SAX Polymers |