Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 110 kJ/m² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 110 kJ/m² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 GR45 NL HS PA6, 45% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 110 kJ/m² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural Information provided by Eurotec® |