Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 52.0 kJ/m²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched (ISO) 52.0 kJ/m²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Izod Impact, Unnotched (ISO) 52.0 kJ/m²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
Izod Impact, Unnotched (ISO) 52.0 kJ/m²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 52.0 kJ/m²

@Temperature -40.0 °C
24.7 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Verton RV006ESV_GY7E071 PA 66
Preliminary Data for 30% long glass fiber, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 52.0 kJ/m²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX103R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r..
Izod Impact, Unnotched (ISO) 52.0 kJ/m²

@Temperature -30.0 °C
24.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..