Polymer Property : Izod Impact, Unnotched (ISO) = 44.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 44.0 kJ/m²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 180/1U
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Izod Impact, Unnotched (ISO) 44.0 kJ/m²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Izod Impact, Unnotched (ISO) 44.0 kJ/m²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled
SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 44.0 kJ/m²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled
SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers