Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 44.0 kJ/m² @Temperature 23.0 °C |
20.9 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180/1U |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Izod Impact, Unnotched (ISO) | 44.0 kJ/m² @Temperature 23.0 °C |
20.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Izod Impact, Unnotched (ISO) | 44.0 kJ/m² @Temperature 23.0 °C |
20.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 44.0 kJ/m² @Temperature 23.0 °C |
20.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers |