Polymer Property : Izod Impact, Unnotched (ISO) = 4.28 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 9.00 kJ/m²

@Thickness 4.00 mm,
Temperature -20.0 °C
4.28 ft-lb/in²

@Thickness 0.157 in,
Temperature -4.00 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Izod Impact, Unnotched (ISO) 9.00 kJ/m²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 9.00 kJ/m²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 180/1U
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 9.00 kJ/m²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1U
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 9.00 kJ/m²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
80x10x4; ISO 180/1U
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.