Izod Impact, Unnotched (ISO) 330 kJ/m²

@Temperature 23.0 °C
157 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1U
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers