Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 54.0 kJ/m² @Temperature 23.0 °C |
25.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1eA |
Polyplastic Armlen® PP GF 30-5HS-901 Polypropylene, 30% Glass Filled Heat stabilized, black colorInformation provided by PolyPlastic Group. |