Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 48.0 kJ/m²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Sax Polymers SAXAMID 226F5RY01 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5RY01 is a polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has a halogen-free flame retardant and UL listed.Information provided by SAX Polymers