Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Thickness 4.00 mm, Temperature -20.0 °C |
9.52 ft-lb/in² @Thickness 0.157 in, Temperature -4.00 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1393 Conductive Thermoplastic Compound PRE-ELEC® PP 1393 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity,.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 kJ/m² @Temperature 0.000 °C |
9.52 ft-lb/in² @Temperature 32.0 °F |
Phr = 5 |
Shandong Rike Chemical HELIâ„¢ HL-35 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |