Polymer Property : Izod Impact, Unnotched (ISO) = 15.2 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS
Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East)
VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Sax Polymers SAXALEN PPC343G20 Polypropylene Copolymer, 20% Glass Filled
SAXALEN PPC343G20 is a 20% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers
Izod Impact, Unnotched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East)
VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
Izod Impact, Unnotched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East)
VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd..